如何验收环氧地坪工程?环氧地坪验收标准
验收环氧地坪工程具体内容:1.打磨清理待修补部分地面;质量要求及验收标准:凡是待修补地面部分,均应该露出水泥地面的新鲜层或旧涂层的新鲜层,以保证所施工环氧底涂与原地面有良好的粘结力;打磨完后应该将待施工地面灰尘杂物清理干净。
Specific contents of acceptance and acceptance of epoxy flooring project: 1. grinding and cleaning parts of the ground to be repaired; quality requirements and acceptance criteria: all parts of the ground to be repaired should expose the fresh layer of the cement floor or the fresh layer of the old coating, in order to ensure that the eptance of the construction eptance of epoxy primer and the original good bonding force of the ground; after grinding, the construction should be completed. Clean up dirt and dust.
2.高渗透性环氧树脂底油一遍,自然固化;(底涂)
2. high permeable epoxy resin base oil, solidified naturally; (primer)
质量要求及验收标准:滚涂底油时应使其涂层均匀,无漏涂;底油完全固化后应形成一层透明的环氧树脂涂层。
Quality Requirements and Acceptance Standards: When rolling the base oil, the coating should be uniform and leak-free; after the base oil is completely cured, a transparent epoxy resin coating should be formed.
3.以环氧树脂中涂材料镘刮一遍,自然固化;(中涂)
3., the epoxy resin coated material is scraped and naturally cured.
质量要求及验收标准:根据修补层的厚度确定要加入石英砂的粗细(50-100目),该砂浆层一次施工厚度最好不应超过2mm。砂浆层施工完毕后应让其完全固化后方能施工下一道工序。中涂完全固化的标准为:受到重压后不会出现凹陷。
Quality requirements and acceptance criteria: According to the thickness of repairing layer, the thickness of quartz sand (50-100 mesh) should be added, and the thickness of the mortar layer should not exceed 2 mm at a time. Mortar layer should be completely solidified after construction, and then the next process can be constructed. The standard for complete curing is: no dents will be felt after heavy pressure.
4.打磨机打磨中涂层;
4. grinding machine to polish the coating;
质量要求及验收标准:要求打磨后的砂浆层平整,平滑,表面无凸起。
Quality requirements and acceptance criteria: the required mortar layer is smooth and smooth without surface bulging.
5.双组分环氧树脂自流平面涂料按比例调配,镘刀施工自然固化(面涂)
5. two-component epoxy self flow flat coating is proportionally distributed, and the construction of the trowel is naturally solidified (surface coating).
质量要求及验收标准:施工面涂之前必需保证地面清洁,表面不能有砂粒、杂物等;施工车间厂房要求完全封闭。
Quality Requirements and Acceptance Standards: Before painting the construction surface, it is necessary to ensure that the ground is clean, and the surface should not contain sand, sundries, etc. The workshop should be completely closed.
6.养护
6. maintenance
质量要求及验收标准:封闭场地,严禁行人行车,表面不得洒落杂物等。
Quality requirements and acceptance criteria: closed space, no pedestrians driving, no surface debris.
验收环氧地坪工程技术指标:
Acceptance of epoxy floor engineering technical indicators:
干燥时间 表干 ≤4
Drying schedule is less than 4.
实干 ≤24
Actual work is less than 24
附着力(级) ≤1
Adhesion force (grade) is less than 1
铅笔硬度 ≥2H
Pencil hardness is more than 2H
耐冲击性 50通过
Impact resistance 50 passes
柔韧性 1㎜通过
Flexibility 1 pass
耐磨性(750g/500R,失重g)≤0.03
Wear resistance (750g/500R, weightlessness g) is less than 0.03.
耐水性 48小时无变化
No change in water resistance for 48 hours.
耐30%硫酸 7天无变化
Resistant to 30% sulfuric acid for 7 days without change.
耐40%氢氧化钠 7天无变化
40% NaOH resistant for 7 days without change.
耐汽油 120# 7天无变化
Gasoline resistant 120# remained unchanged for 7 days.
耐润滑油 7天无变化
No change in lubricating oil for 7 days.
环氧地坪工程验收标准:
Acceptance criteria for epoxy floor project:
1、环境温度为25℃时,施工后2-3天应达到实干,即硬度达到完成固化的80%左右;
1. When the ambient temperature is 25 C, the hardness should reach about 80% of the solidification after 2-3 days of construction.
2、表面不能出现发粘现象;
2, the surface can not appear sticky phenomenon;
3、气泡:平涂型、砂浆型无气泡,自流平允许1个小气泡/10平方米;
3, bubble: flat coated, mortar type no bubbles, self leveling allows 1 small bubbles /10 square meters;
4、流平性好,无镘刀痕,大面积接口处基本平整;
4, good leveling, no trowel marks, large area of the interface is basically smooth.
5、无浮色发花,颜色均匀一致,大面积接口处允许有极不明显的色差;
5, no floating color and flower, uniform color, large area interface allows very insignificant chromatic aberration;
6、无粗杂质,但允许有空气中的 浮尘掉落在造成的极小缺陷;
6, there is no coarse impurity, but it allows the floating dust in the air to drop into the minimal defect.
7、环氧地坪表面应平整平滑,光泽度应达到设计要求(高光泽≥90、有光≥70、半光50~70),平涂型为有光、水性为半光~无光;
7. The surface of the floor should be smooth and smooth, and the glossiness should meet the design requirements (high gloss (> 90), gloss (> 70), half gloss (> 50-70). The flat coating type should be glossy and water-based should be half glossy (~dull).
8、桔皮、砂浆防滑面效果应很明显。
8, orange peel and mortar anti slip surface effect should be very obvious.
上一篇:环氧地坪破损了该怎么修补呢?
下一篇:怎样保养环氧地坪才能延长地坪使用寿命?
- 工厂车间为什么要花钱安装环氧地坪?11-04
- 行业菜鸟选择环氧地坪涂料的方法?【必读】11-03
- 环氧地坪厂家教您如何处理地坪表面不平整11-03
- 厂家揭示寒冷天气该如何施工环氧地坪漆11-01
- 环氧地坪漆工程硬度不好有哪几方面原因11-01
无锡.惠山区.搬家公司 |
无锡.堰桥.搬家公司 | 无锡.前洲.搬家公司
| 无锡.玉祁.搬家公司 | 无锡.洛社.搬家公司
| 无锡.钱桥.搬家公司 | 无锡.阳山.搬家公司
| 无锡.锡山区.搬家公司 | 无锡.东亭.搬家公司
| 无锡.安镇.搬家公司 | 无锡.羊尖.搬家公司
| 无锡.鸿山.搬家公司 | 无锡.鹅湖.搬家公司
| 无锡.东北塘.搬家公司 | 无锡.锡北.搬家公司
| 无锡.东港.搬家公司 | 无锡.滨湖区.搬家公司
| 无锡.河埒.搬家公司 | 无锡.荣巷.搬家公司
| 无锡.蠡湖.搬家公司 | 无锡.蠡园.搬家公司
| 无锡.太湖.搬家公司 | 无锡.华庄.搬家公司
| 无锡.滨湖.搬家公司 | 无锡.马山.搬家公司
| 无锡.胡埭.搬家公司 | 无锡.旺庄.搬家公司
| 无锡.南站.搬家公司 | 无锡.硕放.搬家公司
| 无锡.坊前.搬家公司 | 无锡.梅村.搬家公司
| 无锡.北塘区.搬家公司 | 无锡.黄巷.搬家公司
| 无锡.山北.搬家公司 | 无锡.北大街.搬家公司
| 无锡.惠山.搬家公司 | 无锡.南长区.搬家公司
| 无锡.长街.搬家公司 | 无锡.迎龙桥.搬家公司
| 无锡.谈渡桥.搬家公司 | 无锡.通扬桥.搬家公司
| 无锡.清扬路.搬家公司 | 无锡.清名桥.搬家公司
| 无锡.中桥.搬家公司 | 无锡.芦庄.搬家公司
| 无锡.扬名.搬家公司 | 无锡.崇安区.搬家公司
| 无锡.崇安寺.搬家公司 | 无锡.通江.搬家公司
| 无锡.广瑞路.搬家公司 | 无锡.上马墩.搬家公司
| 无锡.江海.搬家公司 | 无锡.广益.搬家公司 |
最新文章
推荐文章
-
无锡搬家公司一般是
无锡搬家公司一般是怎么收费的?楼......
-
居民搬家时搬运冰
居民搬家时搬运冰箱需要注意事项......
-
搬家时针对特殊物品
特别物品搬运搬迁指导:搬家时一定......
-
搬家时必须晓得的风
搬家可是一件大事,其中的讲究也是......
-
搬家禁忌都有什么/搬
搬家风水1:搬家当天尽量说些吉祥......
热门文章
-
家庭保洁服务项目包
家庭保洁服务项目包括哪些内容?通......
-
怎么辨别无锡搬家公
怎么辨别无锡公司搬家哪家好、个......
-
搬家自己动手拆装空
搬家自己动手拆装空调的方法及注......
-
2016年搬家禁忌及
2016年搬家禁忌及化解1、对于201......
-
搬家前以及过程中
搬家前以及过程中应该注意的事项......
网友评论
家庭保洁服务项目包括哪些内容?
家庭保洁服务项目包括哪些内容?通过专业保洁人员使用清洁设备、工具和药剂,对居室内地面、墙面、顶棚、阳台、厨房、卫生间等部位进行清扫保洁:对门窗、玻璃、灶具、洁具、家具等进行针对性的处理,以达到环 详细>>
搬家公司浅谈家政行业的发展及前景
无锡搬家公司谈谈家政未来的发展 家政服务是改革开放以来,城市经济的繁荣,城市建设高速发展,城市社区的兴起以及居民生活需求内容不断扩大而产生的一个新生行业。根据劳动保障部培训就业司在天津、上海、重 详细>>
住宅小区物业管理经费的主要来源
住宅小区物业管理经费的主要来源:1.定期收取物业管理服务费;2.小区维修养护专项基金;3.以业养业,一业为主,多种经营的收入;4.靠政府多方面的支持;5.开发建设单位给予一定的支持。物业管理对物业的基本要求是 详细>>
花卉租赁公司对用花单位的租摆服务细则
花卉租赁公司对用花单位的租摆服务细则:1、负责花卉的挑选、运输,并摆放在指定地点。2、在租摆期间,花卉租赁公司派专业护花人员每周一次对花卉进行管理,浇水、施肥、病虫害防治、修剪整形、清洁叶片等,用花 详细>>
环氧地坪破损了该怎么修补呢?
环氧地坪是一种装饰和功能都极为良好的一种地面,但是由于使用、保养、施工、使用年限等一些原因会使环氧地坪出现破损的情况一般的东升环氧地坪破损原因有以下几个方面: 详细>>