admin 发表于:2018-10-28 10:40:19   | 只看该作者 查看该作者主题 楼主 

1、温度太低或温度太高,未完全反应.环氧地坪漆施工适合在气温在5℃以上、相对湿度在85%以下进行。如果温度太低,相对湿度太高同样也会出现不干现象,因为5℃以下助剂已经失去活性,这个时候刷环氧地坪漆加没加助剂都是一样。

1. The temperature is too low or too high to react completely. The epoxy floor paint is suitable for the application of the temperature above 5 C and the relative humidity below 85%. If the temperature is too low, the relative humidity is too high will also occur non-drying phenomenon, because the assistant below 5 degrees Celsius has lost activity, this time brush epoxy floor paint with or without additives are the same.

2、主剂和硬化剂配比有误,或未加硬化剂

2. The proportion of main agent and hardener is incorrect or no hardener is added. 在使用环氧地坪漆前没有配比正确,正常来说在使用时候一定要配合其他助剂的,并且严格遵守厂家的配比比例,同时施工人员必须查看涂料产品上的配比标签;助剂加多加少都会造成不干的现象,特别是在施工环氧自流平地坪的配料的时候最好使用电子秤,保证精准。

Before using epoxy floor paint, there is no correct proportion. Normally, other additives must be used in conjunction with other additives, and strictly adhere to the proportion of manufacturers, while the builder must check the paint products on the proportion label; additives more or less will cause non-drying phenomenon, especially in the construction of epoxy self-leveling ground. It is better to use electronic scales to ensure accuracy.

3、硬化剂有误

3. Hardening agent is wrong.

可能是硬化剂的问题,在施工前要选择检查好。

It may be a sclerosing agent. Check before construction.

4、主剂和硬化剂混合时未搅拌均匀

4. The main agent is not stirred even when it is mixed with hardener.

可能在重庆环氧环氧地坪漆施工前搅拌不均匀,这样很容易出现不干的现象,因此一定要进行均匀搅拌。

It is possible that the mixing of epoxy floor paint in Chongqing is not uniform before the construction, so it is easy to occur non-drying phenomenon, so it must be uniform mixing.